The unit price of polipol 321 zero shrink molding polyester resin is calculated over kilograms and sold according to the weight of the package presented. The price offered before packaging selection is the price of the smallest packaging including VAT. The price appears automatically according to your package selection.
product description
Polipol 321-zero is a thixotropic, zero shrinkage unsaturated polyester resin containing accelerator, filler and designed for rapid mold manufacturing. Polipol 321-zero eliminates the appearance of fiber traces that may occur behind the gelcoat, allowing brighter and glass-like surfaces to be obtained. Due to its special accelerator formulation, it quickly hardens and completes its curing. It does not encounter problems such as rotation, shrinkage, etc. in molds. pull is zero. therefore, it fits the model dimensions 100%. It is designed for serial mold making, unlike classical mold polyester, it does not require waiting between layers and saves up to 80% of labor and time. It significantly reduces emission rates with its low styrene rate and LSE structure. It is the ideal lamination resin for producing glossy, mirror-like molds.
recommended areas of use: zero shrinkage formwork system. For special applications where chemical resistance and high thermal resistance are required, please contact the technical team.
application: hand lay-up, fiber-spraying is recommended
shelf life and storage condition: Shelf life is 6 months from the date of manufacture. There is production and expiry date information on each product packaging. polyester resins contain styrene. Styrene is a volatile chemical. All polyester resins should be stored tightly closed, at room temperature (18°C - 26°C), out of direct sunlight. It should be noted that after the package is opened, the shelf life will be shorter than 6 months due to contact with air.
ease of use: suitable for professional and hobby use. (Observe the safety warnings.)
Odor and Appearance: Light yellowish translucent liquid with a strong styrene-based odor.
mixing ratio
Since it contains an accelerator, it is sufficient to add only mekperoxide when using it. Depending on the ambient temperature and the required pot life, 1-2% of its weight mek-p (hardener) is added to the resin for curing at 20-25 °C. Mix thoroughly for 2-3 minutes until the mixture becomes homogeneous. The material is ready to use. It is recommended to dose the cobalt and MEK-P chemicals with the help of a pasteur pipette, MEK-P measuring cups and sensitive scales.
important: always use separate vessels and separate stir bar for cobalt (accelerator) and mek-p (hardener) measurements. When these two chemicals come together in pure form, they are explosive and flammable.
Filling usage: Polipol 321 mold polyester resin is not very suitable for adding filler, it should be kept at a minimum level as the increase in the usage rate of the filling material will increase the risk of fragility of the composite part. It is very important that fillers of different diameters are used together in order to reduce cracks in the product and the shrinkage effect of polyester, and that the filling material does not absorb moisture. Another point to be noted is; Mek-p required for curing should be added to the resin after the filler addition.
Coloring: The surface brightness, color and surface strength of the composite part are provided by gelcoat. If gelcoat production is not to be made, pigment paste is used to color the resins according to the purpose of use. The pigment should be thoroughly mixed with the cobalt added polyester resin, and mek-p (hardener) should be added after deaeration. (See the pigment pastes table for the usage rate.)
Pot life: Pot life varies according to the reactivity of the resins. After adding mek-p to the polyester resin, proceed to the application as quickly as possible. Pot life for all polyester resins is generally 8-12 minutes at 23 °C after adding mek-p (hardener). make sure you use your resin before this time. The curing reactions of polyester resins are exothermic (exothermic). The resin mixed in the container heats up quickly and may even ignite. never leave mek-p and cobalt added resin unattended.
gelling time: (it is the time for the resin viscosity to rise up to a certain point during curing, to reach a jelly consistency). the resin should be brought to its final shape on the mold during this time. gel time: 25-45 min. is.
curing time: (after the accelerator and hardener are added to the polyester resin, it is the time the mixture completes the exothermic curing reaction and turns into a chemically stable and physically hard structure) Average curing time of polipol 321-zero zero shrink molding polyester resin: 25-30 min. filler and pigment Its use prolongs the curing time.
security alert
As with all chemicals, read the product safety warning and file in detail. Points to be considered while using this product; cobalt (accelerator) and mek-p (hardener) are not in direct contact. If they come into contact with each other, the combination is flammable, combustible, explosive. Never use metal measuring cups for both chemicals. (You can examine the mek-cobalt dosing cups on our website.) Do not use the same measuring cup for two chemicals. Do not keep it near the heat source. Wear gloves, safety glasses and work in a well-ventilated area. Never smoke in the working environment. It is recommended that you keep the resin remaining in the mixing bowl after your application in a bowl filled with water until it is fully cured due to the exotherm heat, in this way the negative effects that may occur due to overheating are prevented. Never forget these warnings. When you buy this product, it is assumed that you have read the safety warnings and file and used it according to the written precautions.

IMPORTANT: The information on this website has been prepared with the long-term laboratory tests and institutional knowledge of the manufacturers. KP Composite Pazar A.Ş and the manufacturer are not responsible for any damages arising from the use of this information, which is given as a guide in good faith . KP Composite Pazar A.Ş and the manufacturer cannot be held responsible for problems and damages caused by user errors . We also strongly remind you that before you start using our products in production, you should make application trials in your working environment.